Results
Table 7: Compressibility Testing Results
The results from our strength testing are shown in the following Table 7.
Table 8: Averages and Standard Deviations
Since the minimum standard for strength is generally considered 50 PSI, this indicates that Binder 2 does not meet standards to be used
These are the concentration results of lead and arsenic we got when we XRF the Pilgrim mine tailings after collection.
Table 9: XRF for Pilgrim Mine Site
Table 10: XRF for Magma Mine Site
These are the concentration results of lead and arsenic we got when we XRF the Magma mine tailings after collection.
Table 11: Results from Western Tech Analysis
We are currently waiting on results from Western Tech to finish the table regarding the concentration of heavy metals.